Examples of lithium intercalating mixed oxides containing Ni, Al and at least one second transition metal mixed oxides are compounds of formula Li[NihCoiAlj]O2
wherein
h is 0.7 to 0.9, preferred 0.8 to 0.87, and more preferred 0.8 to 0.85;
i is 0.15 to 0.20; and
j is 0.02 to 10, preferred 0.02 to 1, more preferred 0.02 to 0.1, and most preferred 0.02 to 0.03.
The cathode may further comprise electrically conductive materials like electrically conductive carbon and usual components like binders. Compounds suited as electrically conductive materials and binders are known to the person skilled in the art. For example, the cathode may comprise carbon in a conductive polymorph, for example selected from graphite, carbon black, carbon nanotubes, graphene or mixtures of at least two of the aforementioned substances. In addition, the cathode may comprise one or more binders, for example one or more organic polymers like polyethylene, polyacrylonitrile, polybutadiene, polypropylene, polystyrene, polyacrylates, polyvinyl alcohol, polyisoprene and copolymers of at least two comonomers selected from ethylene, propylene, styrene, (meth)acrylonitrile and 1,3-butadiene, especially styrene-butadiene copolymers, and halogenated (co)polymers like polyvinylidene chloride, polyvinyl chloride, polyvinyl fluoride, polyvinylidene fluoride (PVdF), polytetrafluoroethylene, copolymers of tetrafluoroethylene and hexafluoropropylene, copolymers of tetrafluoroethylene and vinylidene fluoride and polyacrylonitrile.