FIG. 2a): Cycling retention of LiNi0.5Mn1.5O4/Graphite cells (C/5, cutoff potentials at 25° C. and 45° C. 4.80 V?4.25 V vs. LiC6/C6) using the baseline electrolyte without (squares) or with 0.1 wt.-% 2-VP SO3 (circles).
FIG. 2b): Coulombic efficiency of LiNi0.5Mn1.5O4/Graphite cells (C/5, cutoff potentials at 25° C. and 45° C. 4.80 V?4.25 V vs. LiC6/C6) using the baseline electrolyte without (squares) or with 0.1 wt.-% 2-VP SO3 (circles).
FIG. 3a): Cycling retention of LiNi0.5Mn1.5O4/Graphite cells (C/5, cutoff potentials at 25° C. and 45° C. 4.80 V?4.25 V vs. LiC6/C6) using the baseline electrolyte without (squares) or with 0.1 wt.-% 3-FP SO3 (circles).
FIG. 3b): Coulombic efficiency of LiNi0.5Mn1.5O4/Graphite cells (C/5, cutoff potentials at 25° C. and 45° C. 4.80 V?4.25 V vs. LiC6/C6) using the baseline electrolyte without (squares) or with 0.1 wt.-% 3-FP SO3 (circles).
FIG. 4a): Cycling retention of LiNi0.5Mn1.5O4/Graphite cells (C/5, cutoff potentials at 25° C. and 45° C. 4.80 V?4.25 V vs. LiC6/C6) using the baseline electrolyte without (squares) or with 0.1 wt.-% 2-TFP SO3 (circles).