Although there is no particular limitation on the method of manufacturing the interlayer 13, examples thereof include a method in which a resin component, such as the above-described polyvinyl acetal resin, a plasticizer, and other additives, if necessary, are mixed and uniformly kneaded, and then the layers are collectively extruded, and a method in which two or more resin films that are produced using this method are laminated with a pressing process, a lamination process, or the like. In the method of laminating with the pressing process, the lamination process, or the like, each of the resin films before laminating may have a single-layer structure or a multilayer structure. Also, the interlayer 13 may include a single layer instead of the plurality of layers as mentioned above.
2. Overview of Blocking Layer
Next, the blocking layer 4 will be described. As shown in